[1]李富民,袁迎曙.锈蚀钢绞线的静力拉伸断裂特性[J].东南大学学报(自然科学版),2007,37(5):904-909.[doi:10.3969/j.issn.1001-0505.2007.05.033]
 Li Fumin,Yuan Yingshu.Fracture behaviour of corroded steel strands under static tension[J].Journal of Southeast University (Natural Science Edition),2007,37(5):904-909.[doi:10.3969/j.issn.1001-0505.2007.05.033]
点击复制

锈蚀钢绞线的静力拉伸断裂特性()
分享到:

《东南大学学报(自然科学版)》[ISSN:1001-0505/CN:32-1178/N]

卷:
37
期数:
2007年第5期
页码:
904-909
栏目:
材料科学与工程
出版日期:
2007-09-20

文章信息/Info

Title:
Fracture behaviour of corroded steel strands under static tension
作者:
李富民 袁迎曙
中国矿业大学建筑工程学院, 徐州 221008
Author(s):
Li Fumin Yuan Yingshu
College of Architecture and Civil Engineering,China University of Mining and Technology, Xuzhou 221008,China
关键词:
预应力混凝土 耐久性 钢绞线 锈蚀 断裂 扫描电镜 珠光体位向
Keywords:
prestressed concrete durability steel strand corrosion fracture scanning electron microscope orientation of pearlites
分类号:
TU511.3
DOI:
10.3969/j.issn.1001-0505.2007.05.033
摘要:
通过制作专门的掺盐预应力混凝土构件获取锈蚀钢绞线试样,借助宏观观察和微观电镜扫描手段研究了试样的静力拉伸断裂特性,分析了锈蚀对钢绞线静力拉伸断裂特性的影响问题.研究结果表明:当钢绞线钢丝锈蚀坑底部珠光体团的位向与钢丝纵轴线间的夹角较小时,会形成延性的铣刀式断口或杯锥式断口; 反之,当该夹角较大时,会形成脆性的劈裂式断口或劈裂-铣刀式断口; 钢绞线钢丝锈蚀坑处珠光体团的位向是一个概率问题,钢绞线的总体锈蚀程度越大,锈蚀坑与上述夹角较大珠光体团相遇的概率也越大,钢丝出现脆性断裂的概率也越大,整根钢绞线的脆性断裂特征也越明显.
Abstract:
The specimens of corroded steel strands were proposed by purposemade prestressed concrete members mixed with salt. With these specimens, the fracture behavior under static tension was studied by marcro- and microscopic investingation. The influence of corrosion on the fracture behavior under static tension is also discussed. The investigation results show that firstly when the angles between the orientation of pearlites in the corrosion pits and the longitudinal axis of the wires are small, the fractures are ductile and in fraise-mode or cup-mode; whereas, when the angles are large, the fractures are brittle and in cleavage-mode or cleavage-fraise-mode. Secondly, it is a probabilistic affair of the orientation of pearlites in the corrosion pits. With more degree of corrosion, the probability of corrosion pits meeting the pearlites with large angles is more, the probability of brittle fracture of wires is more, and the brittle fracture character of steel strand is clearer.

参考文献/References:

[1] 中国土木工程学会.CCES 01—2004混凝土结构耐久性设计与施工指南[S].北京:中国建筑工业出版社,2005.
[2] Schupack M.A survey of the durability performance of post-tensioning tendons[J]. ACI Journal,1978,75(10):501-510.
[3] Walter P J.Corrosion of prestresing steels and its mitigation[J].PCI Journal,1992(5):34-55.
[4] 郑亚明,欧阳平,安琳.锈蚀钢绞线力学性能的试验研究[J].现代交通技术,2005(6):33-36.
  Zheng Yaming,Ouyang Ping,An Lin.Study on the test of mechanical properties of corroded steel bar embedded in concrete[J]. Modern Technique of Communication,2005(6):33-36.(in Chinese)
[5] 刘其伟,张鹏飞,赵佳军.PC连续梁桥孔道压浆调查及钢绞线力学性能研究[J].施工技术,2007,36(2):63-66.
  Liu Qiwei,Zhang Pengfei,Zhao Jiajun.Duct grouting investigation and research on mechanical properties of steel strand in PC continuous bridges[J]. Construction Technology,2007,36(2):63-66.(in Chinese)
[6] Vehovar L,Kuhar V,Vehovar A.Hydrogen-assisted stress-corrosion of prestressing wires in a motoway viaduct [J]. Engineering Failure Analysis,1998,5(1):21-27.
[7] Valiente A.Stress corrosion failure of large diameter pressure pipelines of prestressed concrete [J]. Engineering Failure Analysis,2001,8(3):245-261.
[8] 戴品强,何则荣,毛志远.珠光体裂纹萌生与扩展的TEM 原位观察[J].材料热处理学报,2003,24(2):41-45.
  Dai Pinqiang,He Zerong,Mao Zhiyuan.In situ TEM observation of crack initiation and propagation in pearlite[J]. Transactions of Materials and Heat Treatment,2003,24(2):41-45.(in Chinese)
[9] Toribio J,Ayaso F J.Anisotropic fracture behaviour of cold drawn steel:a materials science approach[J]. Materials Science and Engineering A,2003,343(1/2):265-272.
[10] Toribio J,Valiente A.Failure analysis of cold drawn eutectoid steel wires for prestressed concrete[J].Engineering Failure Analysis,2006,13(3):301-311.
[11] 李富民,袁迎曙.氯盐环境下混凝土内钢绞线的锈蚀特性试验研究[J].铁道科学与工程学报,2006,3(4):23-28.
  Li Fumin,Yuan Yingshu.Corrosion behaviour of steel strand in concrete under chloride environment[J].Journal of Railway Science and Engineering,2006,3(4):23-28.(in Chinese)

相似文献/References:

[1]李富民,袁迎曙,杜健民,等.氯盐腐蚀钢绞线的受拉性能退化特征[J].东南大学学报(自然科学版),2009,39(2):340.[doi:10.3969/j.issn.1001-0505.2009.02.028]
 Li Fumin,Yuan Yingshu,Du Jianmin,et al.Deterioration of tensile behavior of steel strands corroded by chloride[J].Journal of Southeast University (Natural Science Edition),2009,39(5):340.[doi:10.3969/j.issn.1001-0505.2009.02.028]
[2]王国林,孟少平,张运涛,等.基于改进拉-压杆模型的预应力混凝土深受弯构件受剪承载力预测[J].东南大学学报(自然科学版),2007,37(5):898.[doi:10.3969/j.issn.1001-0505.2007.05.032]
 Wang Guolin,Meng Shaoping,Zhang Yuntao,et al.Prediction of shear capacity of prestressed concrete deep flexural members based on modified strut-and-tie model[J].Journal of Southeast University (Natural Science Edition),2007,37(5):898.[doi:10.3969/j.issn.1001-0505.2007.05.032]
[3]董朝文,于百勇,陈锁忠.地铁工程中高性能混凝土耐久性综合评估[J].东南大学学报(自然科学版),2006,36(2):267.[doi:10.3969/j.issn.1001-0505.2006.02.018]
 Dong Chaowen,Yu Baiyong,Chen Suozhong.Comprehensive evaluation on durability of high-performance concrete in subway construction[J].Journal of Southeast University (Natural Science Edition),2006,36(5):267.[doi:10.3969/j.issn.1001-0505.2006.02.018]
[4]贡金鑫,王海超,李金波.腐蚀环境中荷载作用对钢筋混凝土梁腐蚀的影响[J].东南大学学报(自然科学版),2005,35(3):421.[doi:10.3969/j.issn.1001-0505.2005.03.021]
 Gong Jinxin,Wang Haichao,Li Jinbo.Effect of loading on corrosion of reinforced concrete beam exposed in corroded environment[J].Journal of Southeast University (Natural Science Edition),2005,35(5):421.[doi:10.3969/j.issn.1001-0505.2005.03.021]
[5]孙晓燕,黄承逵,孙保沭.既有桥梁外贴纤维布加固后可靠度分析[J].东南大学学报(自然科学版),2005,35(3):427.[doi:10.3969/j.issn.1001-0505.2005.03.022]
 Sun Xiaoyan,Huang Chengkui,Sun Baoshu.Time-dependent reliability analysis of existing bridges strengthened with FRP laminates[J].Journal of Southeast University (Natural Science Edition),2005,35(5):427.[doi:10.3969/j.issn.1001-0505.2005.03.022]
[6]涂永明,吕志涛.应力状态下混凝土的碳化试验研究[J].东南大学学报(自然科学版),2003,33(5):573.[doi:10.3969/j.issn.1001-0505.2003.05.008]
 Tu Yongming,Lü Zhitao.Experiment and research of presteressed concrete structure in carbonation corrosive environments[J].Journal of Southeast University (Natural Science Edition),2003,33(5):573.[doi:10.3969/j.issn.1001-0505.2003.05.008]
[7]陆惠民,吕志涛.PPC超静定结构弯矩调幅限值及方法的研究[J].东南大学学报(自然科学版),1999,29(2):70.[doi:10.3969/j.issn.1001-0505.1999.02.014]
 Lu Huimin,Lu Zhitao.Study of Moment Modification of Partially Prestressed Concrete Hyperstatic Structures[J].Journal of Southeast University (Natural Science Edition),1999,29(5):70.[doi:10.3969/j.issn.1001-0505.1999.02.014]
[8]薛伟辰,吕志涛.预应力混凝土门式刚架的抗震性能研究[J].东南大学学报(自然科学版),1995,25(6):74.[doi:10.3969/j.issn.1001-0505.1995.06.014]
 Xue Weichen,Lu Zhitao.Research on Seismic Behavior of Unbonded Prestressed Concrete Structures[J].Journal of Southeast University (Natural Science Edition),1995,25(5):74.[doi:10.3969/j.issn.1001-0505.1995.06.014]
[9]杨建明,吕志涛.预应力混凝土框架顶层边柱的合理设计[J].东南大学学报(自然科学版),1992,22(1):43.[doi:10.3969/j.issn.1001-0505.1992.01.008]
 Yang Jianming,Lu Zhitao.Reasonable Design of Top-Exterior Columns of PC Frames[J].Journal of Southeast University (Natural Science Edition),1992,22(5):43.[doi:10.3969/j.issn.1001-0505.1992.01.008]
[10]杨建明.计算预应力混凝土超静定结构次弯矩的直接法[J].东南大学学报(自然科学版),1991,21(4):59.[doi:10.3969/j.issn.1001-0505.1991.04.010]
 Direct Method of Calculating Secondary Moments in Statically Indeterminate Prestressed Concrete Structures[J].Journal of Southeast University (Natural Science Edition),1991,21(5):59.[doi:10.3969/j.issn.1001-0505.1991.04.010]

备注/Memo

备注/Memo:
基金项目: 国家自然科学基金资助项目(50478100,50538070)、中国矿业大学青年科研基金资助项目(0B060086)、徐州市社会发展基金资助项目(2006-15).
作者简介: 李富民(1972—),男,博士生,副教授,fmli@cumt.edu.cn.
更新日期/Last Update: 2007-09-20