[1]王龙,吴波.盲孔法识别拉(压)弯钢管内力的分析与试验[J].东南大学学报(自然科学版),2009,39(6):1179-1186.[doi:10.3969/j.issn.1001-0505.2009.06.019]
 Wang Long,Wu Bo.Analysis and experimental study on identification of inner force of steel tube under tension(compression)and bending using blind-hole method[J].Journal of Southeast University (Natural Science Edition),2009,39(6):1179-1186.[doi:10.3969/j.issn.1001-0505.2009.06.019]
点击复制

盲孔法识别拉(压)弯钢管内力的分析与试验()
分享到:

《东南大学学报(自然科学版)》[ISSN:1001-0505/CN:32-1178/N]

卷:
39
期数:
2009年第6期
页码:
1179-1186
栏目:
土木工程
出版日期:
2009-11-20

文章信息/Info

Title:
Analysis and experimental study on identification of inner force of steel tube under tension(compression)and bending using blind-hole method
作者:
王龙 吴波
华南理工大学亚热带建筑科学国家重点实验室,广州 510640
Author(s):
Wang Long Wu Bo
State Key Laboratory of Subtropical Building Science,South China University of Technology,Guangzhou 510640,China
关键词:
盲孔法 钢管 识别 应力
Keywords:
blind-hole method steel tube identification stress
分类号:
TU392.3
DOI:
10.3969/j.issn.1001-0505.2009.06.019
摘要:
为了解在役拉(压)弯钢管的内力情况,在盲孔法测量钢结构应力的基础上,提出了拉(压)弯钢管的内力识别方法.采用盲孔法对不同外径、不同荷载下的3组9根钢管试件进行了2种不同方式下的钻孔试验,研究了不同钻孔方式、不同外径、不同表面应力分布情况下的钻孔释放规律.试验结果表明:钻孔加工应变对测量精度影响较大,计算应力时应消除钻孔加工应变的影响; 在应力超过fy/2时需对释放系数进行塑性修正; 钢管表面应力的测量精度随钢管直径的增大而提高.盲孔法用于拉(压)弯钢管的表面应力检测和杆件内力识别,无论理论上还是实际操作都是可行的,识别精度满足工程应用要求.
Abstract:
To find out the inner force of existing steel tube under tension(compression)and bending,a method based on stress measurement of steel structure using blind-hole method is proposed to identify the inner force of the member. Experimental investigations with two different hole-drilling manners were carried out on nine steel tubes of different diameter and loading. The rules of the strain release were studied under different diameters,hole-drilling manners,and distributions of surface stress when the holes were drilled. The experimentation indicates that the measurement precision is greatly influenced by the strains induced by drilling hole(as called drilling strain),the influence of drilling strains should be eliminated when stress is calculated; the strain release factors should be corrected when the stress exceeds fy/2; the measurement precision of the surface stress is improved with the steel tube diameter increasing. Surface stress measuring and inner force identification of steel tube under tension(compression)and bending are practical and feasible by using blind-hole method,and the accuracy can meet the need of the engineering application.

参考文献/References:

[1] Mathar J.Determination of initial stresses by measuring the deformations around drilled holes [J].Tran ASME,1934,56(4):249-254.
[2] Soete W,Vancrombrugge R.An industrial method for the determination of residual stresses [J].Proc SESA,1950,8(1):17-26.
[3] ASTM International.E837 Standard test method for determining residual stresses by the hole-drilling strain-gage method[S].West Conshohocken,PA,USA:ASTM,2002.
[4] 中国船舶工业总公司.GB 3395—92残余应力测试方法钻孔应变释放法[S].北京:中国标准出版社,1992.
[5] 裴怡,包亚峰,唐慕尧.盲孔法测定时计算公式中A,B值的研究[J].机械强度,1997,19(1):18-21.
  Pei Yi,Bao Yafeng,Tang Muyao.Study on the A,B values in calculating formula of blind-hole technique [J].Journal of Mechanical Strength,1997,19(1):18-21.(in Chinese)
[6] 陈怀宁,陈亮山,董秀中.盲孔法测量残余应力的钻削加工应变[J].焊接学报,1994,15(4):276-280.
  Chen Huaining,Chen Liangshan,Dong Xiuzhong.Drilling strains in measuring residual stress with hole-drilling strain-gage method[J].Transactions of the China Welding Institution,1994,15(4):276-280.(in Chinese)
[7] 刘柏梁,焦建强,李广铎.钻孔法测定焊接残余应力时的塑性释放应变[J].大连铁道学院学报,1994:15(2):87-94.
  Liu Bailiang,Jiao Jiangqiang,Li Guangduo.Plastic released strain in determining residual welding stresses by hole-drilling method[J].Journal of Dalian Railway Institute,1994,15(2):87-94.(in Chinese)
[8] 赵海燕,裴怡,史耀武,等.用小孔释放法测量焊接高残余应力时孔边塑性变形对测量精度的影响及修正方法[J].机械强度,1996,18(3):17-26.
  Zhao Haiyan,Pei Yi,Shi Yaowu,et al.The influence and correction to the measuring error of high welding residual stress when using hole-drilling method [J]. Journal of Mechanical Strength,1996,18(3):17-26.(in Chinese)
[9] 潘汉明,孙大海.用钻孔法测定焊接薄壁钢管纵向残余应力[J].四川建筑,2005,25(6):91-93.
  Pan Hanming,Sun Dahai.Determining longitudinal residual stresses of welded thin-walled steel tubes by hole-drilling methods[J]. Shi Chuan Architecture,2005,25(6):91-93.(in Chinese)
[10] Young W C,Budynas R G. Roark’s formulas for stress and strain[M].7th ed.北京:清华大学出版社,2003.

相似文献/References:

[1]谭克锋,蒲心诚.钢管超高强混凝土力学性能的研究[J].东南大学学报(自然科学版),1999,29(4):127.[doi:10.3969/j.issn.1001-0505.1999.04.027]
 Tan Kefeng,Pu Xincheng.A Study on the Mechanical Properties of Steel Tubular Very High-Strength Concrete[J].Journal of Southeast University (Natural Science Edition),1999,29(6):127.[doi:10.3969/j.issn.1001-0505.1999.04.027]
[2]白亮,周天华,谢鹏飞,等.小剪跨比内置钢管组合剪力墙抗震性能试验研究[J].东南大学学报(自然科学版),2017,47(3):545.[doi:10.3969/j.issn.1001-0505.2017.03.022]
 Bai Liang,Zhou Tianhua,Xie Pengfei,et al.Experimental study on seismic behaviors of steel stub filled composite shear walls with low aspect ratio[J].Journal of Southeast University (Natural Science Edition),2017,47(6):545.[doi:10.3969/j.issn.1001-0505.2017.03.022]

备注/Memo

备注/Memo:
作者简介:王龙(1975—),男,博士生,高级工程师; 吴波(联系人),男,博士,研究员,博士生导师,bowu@scut.edu.cn.
基金项目: 教育部新世纪优秀人才支持计划资助项目(NCET-04-0819).
引文格式: 王龙,吴波.盲孔法识别拉(压)弯钢管内力的分析与试验[J].东南大学学报:自然科学版,2009,39(6):1179-1186. [doi:10.3969/j.issn.1001-0505.2009.06.019]