Title:
Properties of nano-zirconia toughened diatomite ceramic for dentistry
作者:
梁慧12 刘梅3 顾宁12 章非敏3
1 东南大学生物科学与医学工程学院, 南京 210096; 2 苏州市生物医用材料与技术重点实验室,苏州 215123; 3 南京医科大学口腔医学研究所,南京 210029
Author(s):
Liang Hui12 Liu Mei3 Gu Ning12 Zhang Feimin3
1 School of Biological Science and Medical Engineering, Southeast University, Nanjing 210096,China
2 Suzhou Key Laboratory of Biomedical Materials and Technology, Suzhou 215123,China
3 Institute of Stomatology, Nanjing Medical University, Nanjing 210029, China
关键词:
纳米氧化锆 硅藻土陶瓷 力学性能 增韧机制
Keywords:
nano-zirconia diatomite ceramic mechanical properties toughening mechanism
分类号:
R783.1
DOI:
10.3969/j.issn.1001-0505.2010.03.038
摘要:
探讨了不同含量纳米氧化锆颗粒对牙科用硅藻土陶瓷的增韧增强作用.在硅藻土陶瓷基体原料中添加纳米氧化锆颗粒(w(ZrO2)=0~30%),复合粉体经球磨、烘干、研磨、过筛后压制成型,然后于1 100 ℃常压高温烧结.制得样品经打磨抛光后采用三点弯曲法和压痕法测试陶瓷的力学性能,并利用X射线衍射仪和扫描电子显微镜分析其物相组成和显微结构.实验结果表明,当w(ZrO2)=20%时,硅藻土陶瓷的增韧效果最为明显,三点抗弯强度提高130%,断裂韧性提高30%,硬度则提高较少.经过纳米氧化锆增强增韧的硅藻土陶瓷满足牙科用全瓷材料性能的基本要求.
Abstract:
The toughening and strengthening effects of different contents of nano-zirconia on diatomite ceramics are investigated. Zirconia nanoparticles are added to the diatomite ceramic matrix materials(w(ZrO2)=0 to 30%). After balling, drying, grinding and riddling, the composite ceramics are pressed by a bead machine, and then the obtained greenwares are sintered under atmospheric pressure at 1 100 ℃. After milling and polishing, the mechanical properties of the sintered samples are tested using the three-point method and the indentation method. The phases and microstructures of the composite ceramics are studied by X-ray diffraction and scanning electron microscope, respectively. The experimental results indicate that when w(ZrO2)=20%, the toughening effect of diatomite ceramic is obvious. Correspondingly, the flexural strength and the fracture toughness increase 130% and 30% respectively, while the hardness increases a little. The nano-zirconia toughened diatomite ceramic meets the basic requirements of dental machinable ceramics.

参考文献/References:

[1] Tsai W T,Lai C W,Hsien K J.Characterization and adsorption properties of diatomaceous earth modified by hydrofluoric acid etching[J].Journal of Colloid and Interface Science,2006,297(2):749-754.
[2] Martinovic S,Vlahhovic M,Bolijanac T,et al.Preparation of filter aids based on diatomites[J].Internal Journal of Mineral Process,2006,80(2/3/4):255-260.
[3] Kaufhold S,Dohrmann R,Ulrichs C.Shelf life stability of diatomites[J].Appl Clay Sci,2008,41(3/4):158-164.
[4] Al-Degs Y,Khraisheh M A M,Tutunji M F.Sorption of lead ions on diatomite and manganese oxides modified diatomite[J].Water Res,2001,35(15):3724-3728.
[5] Christensen A N,Lundtoft B,Madsen I C.Investigation of the formation of cristobalite from the diatomaceous clay moler using powder X-ray diffractometry data and profile refinement methods[J]. J Am Ceram Soc,2001,84(4):878-880.
[6] Li S H,Wijn J R,Layrolle P.Novel method to manufacture porous hydroxyapatite by dual-phase mixing[J].J Am Ceram Soc,2003,86(1):65-72.
[7] Licciulli A,Esposito C,Greco A,et al.Laser stereolithography of ZrO2 toughened Al2O3[J].Journal of the European Ceramic Society,2005,25(9):1581-1589.
[8] Thompson J Y,Stoner B R,Piascik J R.Ceramics for restorative dentistry:critical aspects for fracture and fatigue resistance[J].Materials Science and Engineering,2007,27(3):565-569.
[9] Wolfram H,Volker R,Elke A,et al.Principles and phenomena of bioengineering with glass-ceramics for dental restoration[J].Journal of the European Ceramics Society,2007,27(2/3):1521-1526.
[10] Zhong J,Huang C.Study on ceramic tool material with nano-scale zirconia toughening alumina matrix[J].Tool Engineering,2008,42(10):51-53.
[11] Wang Qi,Chen Qiang,Zhu Jianguo,et al.Effects of pore shape and porosity on the properties of porous LNKN ceramics as bone substitute[J]. Materials Chemistry and Physics,2008,109(2/3):488-491.
[12] 孙义海,张玉峰,郭景坤.低温烧结高性能2Y-TZP材料[J].无机材料学报,2002,17(6):1227-1231.
  Sun Yihai,Zhang Yufeng,Guo Jingkun.Low-temperature sintered high-performance 2Y-TZP materials[J].Journal of Inorganic Materials,2002,17(6):1227-1231.(in Chinese)
[13] Langne F F.Transformation toughening[J].Journal of Materials Science,1982,17(1):225-234.

备注/Memo

备注/Memo:
作者简介: 梁慧(1984—),女,硕士生; 顾宁(联系人),男,博士,教授,博士生导师,guning@seu.edu.cn.
基金项目: 江苏省自然科学基金资助项目(BK2009137).
引文格式: 梁慧,刘梅,顾宁,等.纳米氧化锆增韧牙科用硅藻土陶瓷的性能[J].东南大学学报:自然科学版,2010,40(3):636-639. [doi:10.3969/j.issn.1001-0505.2010.03.038]
更新日期/Last Update: 2010-05-20