[1]钱春香,李瑞阳,潘庆峰,等.混凝土裂缝的微生物自修复效果[J].东南大学学报(自然科学版),2013,43(2):360-364.[doi:10.3969/j.issn.1001-0505.2013.02.025]
 Qian Chunxiang,Li Ruiyang,Pan Qingfeng,et al.Microbial self-healing effects of concrete cracks[J].Journal of Southeast University (Natural Science Edition),2013,43(2):360-364.[doi:10.3969/j.issn.1001-0505.2013.02.025]
点击复制

混凝土裂缝的微生物自修复效果()
分享到:

《东南大学学报(自然科学版)》[ISSN:1001-0505/CN:32-1178/N]

卷:
43
期数:
2013年第2期
页码:
360-364
栏目:
化学化工
出版日期:
2013-03-20

文章信息/Info

Title:
Microbial self-healing effects of concrete cracks
作者:
钱春香李瑞阳潘庆峰罗勉荣辉
东南大学材料科学与工程学院, 南京 211189; 东南大学绿色建材研究所, 南京 211189
Author(s):
Qian Chunxiang Li Ruiyang Pan Qingfeng Luo Mian Rong Hui
School of Materials Science and Engineering, Southeast University, Nanjing 211189, China
Research Institute of Green Construction Materials, Southeast University, Nanjing 211189, China
关键词:
混凝土 裂缝 微生物 自修复 效果
Keywords:
concrete cracks microbial self-healing effect
分类号:
TQl72.1
DOI:
10.3969/j.issn.1001-0505.2013.02.025
摘要:
利用裂缝测宽仪、扫描电镜和热重分析技术分别对混凝土裂缝的微生物自修复效果进行了研究.研究结果表明:修复40 d后,混凝土裂缝就可以被微生物矿化形成的碳酸钙所填充,修复效果明显,最大填充宽度超过1 mm.微生物矿化形成的碳酸钙在裂缝开口处最多,且随着裂缝深度的增加碳酸钙逐渐减少,当混凝土裂缝深度超过10 mm时未发现微生物形成的碳酸钙.距离裂缝断裂面表层1.5 mm内,微生物可矿化形成较多碳酸钙.而当超过1.5 mm时,由于该微生物矿化需要氧气,因此,随着距离裂缝断裂面表层越远、距离水泥基体越近,微生物矿化形成的碳酸钙含量越来越少.
Abstract:
The effect of crack self-healing was studied in bacterial concrete by the crack width gauge, scanning electron microscopy and thermogravimetric analysis. The results indicate that after concrete is cured for 40 d, concrete cracks can be filled with calcium carbonate produced by microbial mineralization. The self-healing effect is obvious and the maximum width is greater than 1 mm. The quantity of calcium carbonate is the largest in the openings of concrete crack. And calcium carbonate is gradually reduced with the increase in the crack depth. When the concrete crack depth is over 10 mm, the formation of calcium carbonate is no longer found. When the distance is less than 1.5 mm, microorganisms can produce a large amount of calcium carbonate through mineralization. However, when the distance is greater than 1.5 mm, the content of calcium carbonate gradually reduces with the increase in the depth. The reason is that the microbial mineralization requires oxygen.

参考文献/References:

[1] Gollapudi U K, Knutson C L, Bang S S, et al. A new method for controlling leaching through permeable channels [J]. Chemosphere, 1995, 30(4): 695705.
[2] Jonkers H M. Self healing concrete: a biological approach[C]//Self Healing MaterialsAn Alternative Approach to 20 Centuries of Materials Science. Springer: The Netherlands, 2007: 195-204.
[3] Jonkers H M, Schlangen E. A two component bacteria-based self-healing concrete [C]//2nd International Conference on Concrete Repair, Rehabilitation and Retrofitting. London: Taylor & Francis Group, 2008: 215-220.
[4] Jonkers H M, Schlangen E. Development of a bacteria-based self healing concrete [C]//Tailor Made Concrete Structures. London: Taylor & Francis Group, 2008: 425-430.
[5] Jonkers H M, Thijssen A, Muyzer G, et al. Application of bacteria as self-healing agent for the development of sustainable concrete [J]. Ecological Engineering, 2010, 36(2): 230-235.
[6] Wiktor V, Jonkers H M. Self-healing of cracks in bacterial concrete[C]//2nd International Symposium on Service Life Design for Infrastructures. Delft, The Netherlands, 2010: 825-831.
[7] Muynck W D, Cox K, Belie N D, et al. Bacterial carbonate precipitation as an alternative surface treatment for concrete[J]. Construction Building Material, 2008, 22(5): 93-103.
[8] Tittelboom K V, Belie N D, Muynck W D, et al. Use of bacteria to repair cracks in concrete[J]. Cement and Concrete Research, 2010, 40(1): 157-166.
[9] de Muynck W, de Belie N, Verstraete W. Microbial carbonate precipitation in construction materials: a review[J]. Ecological Engineering, 2010, 36(2): 118-136.
[10] Rasanen V, Penttala V. The pH measurement of concrete and smoothing mortar using a concrete powder suspension[J]. Cement and Concrete Research, 2004, 34(5):813-820.

相似文献/References:

[1]李富民,袁迎曙,杜健民,等.氯盐腐蚀钢绞线的受拉性能退化特征[J].东南大学学报(自然科学版),2009,39(2):340.[doi:10.3969/j.issn.1001-0505.2009.02.028]
 Li Fumin,Yuan Yingshu,Du Jianmin,et al.Deterioration of tensile behavior of steel strands corroded by chloride[J].Journal of Southeast University (Natural Science Edition),2009,39(2):340.[doi:10.3969/j.issn.1001-0505.2009.02.028]
[2]金祖权,孙伟,侯保荣,等.混凝土的高温变形与微结构演化[J].东南大学学报(自然科学版),2010,40(3):619.[doi:10.3969/j.issn.1001-0505.2010.03.035]
 Jin Zuquan,Sun Wei,Hou Baorong,et al.Deformation and microstructure evolution of concrete subjected to elevated temperature[J].Journal of Southeast University (Natural Science Edition),2010,40(2):619.[doi:10.3969/j.issn.1001-0505.2010.03.035]
[3]王新玲,刘伟,曹双寅.新型复合结构拟静力试验的变形和裂缝[J].东南大学学报(自然科学版),2007,37(6):1036.[doi:10.3969/j.issn.1001-0505.2007.06.019]
 Wang Xinling,Liu Wei,Cao Shuangyin.Deformation and cracks on new compound structure under low-cycle and repeated load[J].Journal of Southeast University (Natural Science Edition),2007,37(2):1036.[doi:10.3969/j.issn.1001-0505.2007.06.019]
[4]潘华,邱洪兴.基于损伤力学的混凝土疲劳损伤模型[J].东南大学学报(自然科学版),2006,36(4):605.[doi:10.3969/j.issn.1001-0505.2006.04.023]
 Pan Hua,Qiu Hongxing.Fatigue model of concrete based on continuum damage mechanics[J].Journal of Southeast University (Natural Science Edition),2006,36(2):605.[doi:10.3969/j.issn.1001-0505.2006.04.023]
[5]耿飞,钱春香.图像分析技术在混凝土塑性收缩裂缝定量测试与评价中的应用研究[J].东南大学学报(自然科学版),2003,33(6):773.[doi:10.3969/j.issn.1001-0505.2003.06.022]
 Geng Fei,Qian Chunxiang.Image analysis technique for quantitative testing and evaluation of plastic shrinkage cracks in concrete[J].Journal of Southeast University (Natural Science Edition),2003,33(2):773.[doi:10.3969/j.issn.1001-0505.2003.06.022]
[6]余红发,孙伟,麻海燕,等.盐湖地区钢筋混凝土结构使用寿命的预测模型及其应用[J].东南大学学报(自然科学版),2002,32(4):638.[doi:10.3969/j.issn.1001-0505.2002.04.023]
 Yu Hongfa,Sun Wei,Ma Haiyan,et al.Prediction model for service life of reinforced concrete structures in salt lakes and its applications[J].Journal of Southeast University (Natural Science Edition),2002,32(2):638.[doi:10.3969/j.issn.1001-0505.2002.04.023]
[7]罗睿,黄晓明,陆原,等.基层对层间连续路面应力强度因子影响的研究[J].东南大学学报(自然科学版),2001,31(3):61.[doi:10.3969/j.issn.1001-0505.2001.03.015]
 Luo Rui,Huang Xiaoming,Lu Yuan,et al.Influence of Base Layer on the Stress Intensity Factor of Pavement with Continual Layers[J].Journal of Southeast University (Natural Science Edition),2001,31(2):61.[doi:10.3969/j.issn.1001-0505.2001.03.015]
[8]田正宏,白凯国,朱静.透水模板布改善混凝土表层质量试验研究[J].东南大学学报(自然科学版),2008,38(1):146.[doi:10.3969/j.issn.1001-0505.2008.01.028]
 Tian Zhenhong,Bai Kaiguo,Zhu Jing.Study on surface quality of concrete improved by infiltrating formwork texture[J].Journal of Southeast University (Natural Science Edition),2008,38(2):146.[doi:10.3969/j.issn.1001-0505.2008.01.028]
[9]钱振东,何长江.钢桥铺面裂缝快速修复材料性能试验研究[J].东南大学学报(自然科学版),2008,38(2):255.[doi:10.3969/j.issn.1001-0505.2008.02.014]
 Qian Zhendong,He Changjiang.Performance test of rapid repair material for cracking on steel deck surfacing[J].Journal of Southeast University (Natural Science Edition),2008,38(2):255.[doi:10.3969/j.issn.1001-0505.2008.02.014]
[10]汪基伟,陈玉泉.平面应变混凝土强度变形试验与等效单轴应变本构模型[J].东南大学学报(自然科学版),2005,35(5):775.[doi:10.3969/j.issn.1001-0505.2005.05.026]
 Wang Jiwei,Chen Yuquan.Strength-deformation test and equivalent uniaxial constitutive model of concrete in plane strain[J].Journal of Southeast University (Natural Science Edition),2005,35(2):775.[doi:10.3969/j.issn.1001-0505.2005.05.026]

备注/Memo

备注/Memo:
作者简介: 钱春香(1966—),女,博士,教授,博士生导师,cxqian@seu.edu.cn.
基金项目: 国家自然科学基金资助项目(51178104)、教育部博士点基金资助项目(20110092110033).
引文格式: 钱春香,李瑞阳,潘庆峰,等.混凝土裂缝的微生物自修复效果[J].东南大学学报:自然科学版,2013,43(2):360-364. [doi:10.3969/j.issn.1001-0505.2013.02.025]
更新日期/Last Update: 2013-03-20