[1]张晋,吴磊,廖家男,等.考虑层板脱落影响的正交胶合木楼板炭化速度试验研究[J].东南大学学报(自然科学版),2019,49(4):705-711.[doi:10.3969/j.issn.1001-0505.2019.04.013]
 Zhang Jin,Wu Lei,Liao Jianan,et al.Experimental study on charring rate of cross-laminated timber floor considering the effect of delamination[J].Journal of Southeast University (Natural Science Edition),2019,49(4):705-711.[doi:10.3969/j.issn.1001-0505.2019.04.013]
点击复制

考虑层板脱落影响的正交胶合木楼板炭化速度试验研究()
分享到:

《东南大学学报(自然科学版)》[ISSN:1001-0505/CN:32-1178/N]

卷:
49
期数:
2019年第4期
页码:
705-711
栏目:
土木工程
出版日期:
2019-07-20

文章信息/Info

Title:
Experimental study on charring rate of cross-laminated timber floor considering the effect of delamination
作者:
张晋1吴磊1廖家男2王卫昌1李维滨1
1东南大学混凝土及预应力混凝土结构教育部重点实验室, 南京211189; 2南宁高新技术产业开发区管理委员会, 南宁530007
Author(s):
Zhang Jin1 Wu Lei1 Liao Jianan2 Wang Weichang1 Li Weibin1
1Key Laboratory of Concrete and Prestressed Concrete Structures of the Ministry of Education, Southeast University, Nanjing 211189, China
2 Organizing Committee of Nanning New & Hi-tech Industry Development Zone, Nanning 530007, China
关键词:
正交胶合木(CLT) 炭化速度 层板脱落 炭化深度计算方法 防火设计
Keywords:
cross-laminated timber(CLT) charring rate delamination charring depth model fire design
分类号:
TU366.2;TU352.5
DOI:
10.3969/j.issn.1001-0505.2019.04.013
摘要:
为研究国产正交胶合木(CLT)楼板受火条件下的层板脱落情况及其对炭化速度的影响,开展了6组试件在给定时间下的炭化速度试验,研究了受火时间、层板厚度和层板脱落对CLT板炭化速度的影响规律,提出了考虑层板脱落影响的炭化深度计算方法.研究结果表明:当CLT楼板受火时间较短、炭化层未发展至层板胶缝处时,未发生层板脱落,其炭化速度与实木、层板胶合木等构件的炭化速度基本相同;当受火时间较长、炭化层发展至层板胶缝处时,采用单组分聚氨酯(PUR)作为胶黏剂压制而成的CLT板将发生层板脱落;且受火时间越长,脱落情况越严重,平均炭化速度越快;对比相同厚度不同层数的CLT板,层板数较多且单层层板厚度较薄的CLT脱落情况更严重,平均炭化速度更快.提出的炭化深度计算方法有效地考虑了受火时CLT楼板层板脱落带来的炭化速度加快的影响,计算结果与试验结果吻合良好,可供工程设计人员参考.
Abstract:
To study the delamination of cross-laminated timber(CLT)floor under fire and its influence on the charring rate, fire tests were carried out on six specimens at different given times. The effects of fire duration, the thickness of CLT floor, and falling off of charred layers on the charring rate of CLT floor were studied. The charring depth calculation method considering the influence of falling off of charred layers was established. The results show that when the CLT floor is exposed to fire within a short time and the char line does not develop to the glue line, the charred layer will not fall off. The charring rate will remain basically the same as that of the solid wood, glue-laminated timber and other engineered timber products. CLT bonded with one-component polyurethane(PUR)adhesive will fall off when the char line develops to the glue line after longer fire exposure. In addition, the longer the fire exposure time, the more serious the falling off and the faster the average charring rate. Compared the results of CLT with different layers, the falling off of the charred layers is found to be more serious and the average charring rate is higher when the number of layers is larger and the lamella is thinner. The proposed charring depth calculation model effectively takes into account the influence of accelerated charring rate caused by falling off of the charred layers under fire. The calculational results are in good agreement with the test ones and can provide a reference for engineers.

参考文献/References:

[1] Karacabeyli E, Douglas B. CLT handbook: Cross-laminated timber[M]. Midison, Canada: FPInnovations and American Wood Council, 2013:1-3.
[2] Frangi A, Fontana M, Knobloch M, et al. Fire behaviour of cross-laminated solid timber panels[J]. Fire Safety Science, 2008, 9: 1279-1290. DOI:10.3801/iafss.fss.9-1279.
[3] Frangi A, Fontana M, Hugi E, et al. Experimental analysis of cross-laminated timber panels in fire[J]. Fire Safety Journal, 2009, 44(8): 1078-1087. DOI:10.1016/j.firesaf.2009.07.007.
[4] Menis A. Fire resistance of laminated veneer lumber(LVL)and cross-laminated timber(XLAM)elements [D]. Cagliari, Italy: Università degli studi di Cagliari, 2012.
[5] Teibinger M, Matzinger I. Basis for evaluation of the fire resistance of timber constructions[R]. Vienna, Austria: Holzforschung Austria Final Report, 2010.
[6] Schmid J, Konig J, Kohler J. Fire-exposed cross-laminated timber—Modelling and tests[C] //World Conference on Timber Engineering. Trentino, Italy: Trees and Timber Institute, 2010.
[7] Fragiacomo M, Menis A, Clemente I, et al. Fire resistance of cross-laminated timber panels loaded out of plane[J].Journal of Structural Engineering, 2013, 139(12): 04013018. DOI:10.1061/(asce)st.1943-541x.0000787.
[8] Buchanan A H. Structural design for fire safety[M]. New York: Wiley, 2001: 280-290.
[9] Drysdale D. An introduction to fire dynamics[M]. Chichester, UK: John Wiley & Sons, Ltd, 2011:318-322.
[10] Lie T T. Structural fire protection[M]. New York: American Society of Civil Engineers, 1992: 38-45.
[11] Bartlett A, Butterworth N, Bisby L A. Fire-induced delamination of cross-laminated timber[C]// European Workshop Fire Safety of Green Buildings. Berlin, Germany, 2015.
[12]American Forest & Paper Association. National design specification for wood construction[S].Washington, DC, USA: American Wood Council, 2018.
[13] British Standards Institution. EN 1995-1-2: 2004, Eurocode5: Design of timber structures, Part 1-2: General—Structural fire design [S]. Brussels, Belgium: European Committee for Standardization,2004.

备注/Memo

备注/Memo:
收稿日期: 2019-01-08.
作者简介: 张晋(1974—),男,博士,教授,博士生导师,zhangjin@seu.edu.cn.
基金项目: 国家重点研发计划资助项目(2017YFC0703503)、 国家自然科学基金资助项目(51778143).
引用本文: 张晋,吴磊,廖家男,等.考虑层板脱落影响的正交胶合木楼板炭化速度试验研究[J].东南大学学报(自然科学版),2019,49(4):705-711. DOI:10.3969/j.issn.1001-0505.2019.04.013.
更新日期/Last Update: 2019-07-20